Active heavy flux.
For soldering even oxidized wires, in the repair of products after exposure to water.
Facilitates soldering of parts made of ferrous and non-ferrous metals.
It is recommended to remove flux residues after soldering with an alcohol-gasoline mixture or another means to remove flux residues.
Attention! Not recommended for soldering multilayer PCBs, high frequency and high voltage devices.
Poorly washed flux residues are electrically conductive and can cause corrosion.
Ingredients:
petroleum jelly (base) 80-90%
paraffin 6-9%
zinc chloride 4-6%
ammonium chloride 1-3%
water 2-4%
weight: 10 g.
packing: tin can.
Only registered users can leave feedback and ask questions
The data presented in the product description are for reference only and may differ from those indicated by the manufacturer.
To carry out technical calculations and obtain the exact parameters of the goods, use the datasheets from the manufacturer's website.
If you need additional information, or you found an error in the description, or have other questions about this product, then our manager will help you: Ярослав
unknown