ЧП Ворон. Электронные компоненты и радиомонтажное оборудование. Микросхемы, транзисторы, реле, резисторы, конденсаторы, паяльное оборудование, припой.
Корзина пуста!
ВХОД ДЛЯ КЛИЕНТОВ

Забыли пароль?
Зарегистрироваться

Шановні клієнти інтернет-магазину!

  У зв'язку зі святкуванням Нового Року ми працюємо за наступним графіком:
• з 31.12.24(Вт) по 02.01.25(Чт) не працюємо
• з 03.01.25(Пт) працюємо в звичайному режимі.

  Інтерет-магазин приймає замовлення цілодобово 24/7 !



Поиск:

Enter a search string or click on the microphone icon and begin speaking.

×
История запросов
ваша история поиска пуста
Whole catalog Materials for production and repairAdhesives, sealants, pastes, scotch tapeConductive adhesives and coatings
Код товара:
019974

Conductive graphite varnish Graphite 200ml [spray]

Colloidal graphite-based conductive varnish. To create and restore a conductive coating in electroplating, when repairing electronic equipment. Spray 200 ml.
Conductive graphite varnish Graphite 200ml [spray]
Manufacturer: CRAMOLIN
NOT available.
Expected price: 516,60 UAH
from 1 pc : 516,60 UAH
from 4 pcs : 490,80 UAH ( -5,0%)
from 12 pcs : 464,90 UAH ( -10,0%)
Prices are indicated at the time of product availability and may change upon receipt

Current balances:

NOT available

Изображение товара

Product description format_size zoom_out zoom_in

The product is easy to apply and adheres firmly to the treated surfaces, including those as smooth as glass. Excellent adhesion to smooth surfaces such as glass and plastics. Remains effective at temperatures up to+300°C.
Coating resistivity 1000-2000 Ohm/m2, depending on the thickness of the applied varnish layer.

Properties:
  • black color
  • density: 0.88 g/cm³
  • interlayer drying time: at room temperature after 10 minutes dries until it comes off
  • complete drying time: after 24 hours dries completely
  • heat resistance: up to+300°С
  • surface resistance: 1000-2000 Ohm/m2

Appointment

  • in preparation for galvanic coating of products made of non-conductive materials to create a surface conductive layer
  • when repairing picture tubes, cathode-ray tubes, it is used to repair damage to the conductive coating of the cone
  • protection against electrostatic discharge 9creation of an equipotential surface).
     
Directions for use

Shake the can well before use. The surface to be protected must be free from dirt and grease.
Spray the aerosol from a distance of approximately 40 cm. Repeat the application two or three times to obtain a thicker layer.
The clogged nozzle is washed with a solvent.

Предлагаемые замены

Leave your feedback or ask a question

Only this product is discussed here. Off topic comments will be deleted! Please follow the Commenting Rules.

The data presented in the product description are for reference only and may differ from those indicated by the manufacturer.
To carry out technical calculations and obtain the exact parameters of the goods, use the datasheets from the manufacturer's website.

If you need additional information, or you found an error in the description, or have other questions about this product, then our manager will help you: Ярослав unknown

Buy with this product: Посмотреть больше…